Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0163 GPa | 2.37 ksi | ASTM D638 |
Colorite Polymers 1194B General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |