Mechanical Properties Metric English Comments
100% Modulus 0.0160 GPa
2.32 ksi
ISO 37
Huntsman AVALON® 98 AE Thermoplastic Polyurethane
Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi..
100% Modulus 0.0160 GPa
2.32 ksi
DIN 53504
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade
Good flow and high mechanical property performance. Suggested for injection molding.Information provided by Huntsman
100% Modulus 0.0160 GPa
2.32 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1600 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..