100% Modulus 0.01568 GPa
2.274 ksi
JIS K6301
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..