Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.012753 GPa | 1.8497 ksi | JIS-K-6723 |
Denka REOMER G G8082 Thermoplastic Elastomer, For Injection Molding Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |