Mechanical Properties Metric English Comments
100% Modulus 0.0111 GPa
1.61 ksi
DIN 53504
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
100% Modulus 0.0111 GPa
1.61 ksi
ISO 37
PolyOne Elastamax XL-0257-1 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color..