Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0107 GPa | 1.55 ksi | ASTM D638 |
Colorite Polymers 8804 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0107 GPa | 1.55 ksi | ASTM D-638 |
Axiall 2110 Wire & Cable Flexible PVC Tray cable jacket for 105°C applications. Also suitable for direct burial applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gu.. |
|||
100% Modulus | 0.0107 GPa | 1.55 ksi | ASTM D-638 |
Axiall 22850 Coax & Telecom Flexible PVC Flexible PVC jacketing compound for coaxial cable and other 75C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0107 GPa | 1.55 ksi | ASTM D-638 |
Axiall 38702 Moldings & Extrusions Flexible PVC Flame retardant CATV and general purpose jacket with excellent low temperature properties. UL approved for 720 hour sunlight resistance in all colors. UL approved for 94 V-0 at 1.5 mm in all color.. |
|||
100% Modulus | 0.0107 GPa | 1.55 ksi | ASTM D-638 |
Axiall 9148 Wire & Cable Flexible PVC Tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0107 GPa | 1.55 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.0107 GPa | 1.55 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
100% Modulus | 0.0107 GPa | 1.55 ksi | ASTM D-638 |
Axiall 38702 Coax & Telecom Flexible PVC Flame retarded CATV and general purpose jacket with excellent low temperature properties. UL approved for 720 hour sunlight resistance in all colors. UL approved for 94 V-0 at 1.5 mm in all colors.. |