Polymer Property : 100% Modulus = 1.475 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.01017 GPa
1.475 ksi
ASTM D-638
Axiall 10840 Wire & Cable Flexible PVC
High gloss jacket and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.01017 GPa
1.475 ksi
ASTM D-638
Axiall 12850 Wire & Cable Flexible PVC
Flame retardant, UV resistant clear compound. Formulated for microbial resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.01017 GPa
1.475 ksi
ASTM D-638
Axiall 12880 Coax & Telecom Flexible PVC
VW-1 coax cable jacket. RG 6.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.01017 GPa
1.475 ksi
ASTM D-638
Axiall 12880 Wire & Cable Flexible PVC
75C general purpose. 720 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.