Polymer Property : 100% Modulus = 1.031 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.007108 GPa
1.031 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer
Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited..