Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00672 GPa | 0.975 ksi | ASTM D-638 |
Axiall 375 Wire & Cable Flexible PVC General purpose and AWM flame retardant jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00672 GPa | 0.975 ksi | ASTM D-638 |
Axiall 16780 Wire & Cable Flexible PVC 90C matte finish, vinyl elastomer.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |