Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00648 GPa | 0.940 ksi | ASTM D-638 |
Axiall 8705 Moldings & Extrusions Flexible PVC General purpose PVC extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |