Mechanical Properties Metric English Comments
100% Modulus 0.00551 GPa
0.799 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00551 GPa
0.799 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00551 GPa
0.799 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FT 2481 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FT 2481 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..