Mechanical Properties Metric English Comments
100% Modulus 0.00526 GPa
0.763 ksi
ASTM D412
Northstar Polymers MPP-A80E High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..