Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00476 GPa | 0.690 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-220 (ISAF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00476 GPa | 0.690 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Mistron Vapor Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00476 GPa | 0.690 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-380A Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00476 GPa | 0.690 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-220 (ISAF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00476 GPa | 0.690 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® 9100 Fluoroelastomer DuPont™ Kalrez® 9100 is an amber translucent product targeted specifically for PECVD and HDPCVD processes. It has also exhibited excellent performance in "select" etch processes. Kalrez® 9100 has.. |
|||
100% Modulus | 0.00476 GPa | 0.690 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2181 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2181 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00476 GPa | 0.690 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Mistron Vapor Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |