Mechanical Properties Metric English Comments
100% Modulus 0.00393 GPa
0.570 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00393 GPa
0.570 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00393 GPa
0.570 ksi
ASTM D412
Teknor Apex UNIPRENE® 7100-73 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00393 GPa
0.570 ksi
ASTM D412
Teknor Apex Uniprene® 73A Polyvinyl Chloride, Flexible
Features: High Elastic RecoveryInformation Provided by Teknor Apex
100% Modulus 0.00393 GPa
0.570 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00393 GPa
0.570 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00393 GPa
0.570 ksi
ASTM D638
Bayshore Vinyl Compounds BVC 7200-65 Vinyl Compound
BVC 7200-65 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s..
100% Modulus 0.00393 GPa
0.570 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00393 GPa
0.570 ksi
ASTM D638
Colorite Polymers 5514 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..