Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00365 GPa | 0.530 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00365 GPa | 0.530 ksi | ASTM D412 |
SK Chemicals SKYTHANE® T875A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00365 GPa | 0.530 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00365 GPa | 0.530 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2123 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2123 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |