Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00234 GPa | 0.339 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00234 GPa | 0.339 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |