Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00144 GPa | 0.209 ksi | |
Colorite Polymers Flexchem 3551-02 Vinyl Compound Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut.. |