100% Modulus 0.00139 GPa
0.201 ksi
Shin-Etsu Silicones SV-15000U Silicone Rubber
SV15000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat..