Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion Information provided by Polykemi AB |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | TPE-0153 (ASTM D 412) |
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D3574E |
Mearthane Durethaneâ„¢ M DM-630A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 500350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 500400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 500450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 600300S SEBS Based Material, Filled Qualities, 30A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 600350S SEBS Based Material, Filled Qualities, 35A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602350S SEBS Based Material, Filled Qualities, 35A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602400S SEBS Based Material, Filled Qualities, 40A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602450S SEBS Based Material, Filled Qualities, 45A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 660300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 660350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 662300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 662350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 662500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Mediprene™ 660440M TPE, Medical Applications, 44A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412 |
3M 550 Polyurethane Adhesive Sealant Fast Cure 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412 |
3M 560 Polyurethane Adhesive Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ISO 37 |
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ISO 37 |
AlphaGary Evoprene™ G 992 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued **)& Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 600500S SEBS Based Material, Filled Qualities, 50A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |