Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000883 GPa | 0.128 ksi | DBPH Cure |
Shin-Etsu Silicones SV-16000U Silicone Rubber SV16000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat.. |