Mechanical Properties Metric English Comments
100% Modulus 0.000724 GPa
0.105 ksi
Mearthane Durethaneâ„¢ F DF-620A Closed Cell Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 65Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
100% Modulus 0.000724 GPa
0.105 ksi
Mearthane Durethaneâ„¢ F DF-235A Closed Cell Foam Polyurethane
TDI backbone: ester.Shore 00 Hardness: 80Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
100% Modulus 0.000724 GPa
0.105 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer
Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and ..