Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000710 GPa | 0.103 ksi | NF T 46-002 |
SMAC SMACTANE® SP Damping Material A viscoelastic rubber material developed by SMAC for space applications and maximizes the damping properties in a wide range of temperatures & frequencies Damping properties: Damping properties are .. |