Polymer Property : 100% Modulus = 0.0660 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.000455 GPa
0.0660 ksi
Mearthane Durethaneâ„¢ F DF-225A Closed Cell Foam Polyurethane
TDI backbone: ester.Shore 00 Hardness: 70Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..