Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000379 GPa | 0.0550 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-720A Solid Polyurethane Elastomer MDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |