Polymer Property : 100% Modulus = 0.0207 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0207 GPa
3.00 ksi
ASTM D412
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
100% Modulus 0.0207 GPa
3.00 ksi
ASTM D-638
Axiall 8571 Moldings & Extrusions Flexible PVC
High quality, semi-rigid extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia ..
100% Modulus 0.0207 GPa
3.00 ksi
ASTM D-638
Axiall 46801 Coax & Telecom Flexible PVC
Semi-rigid flame retardant compound suitable for telecom insulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.