Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0137 GPa | 1.99 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista.. |
|||
100% Modulus | 0.0137 GPa | 1.99 ksi | ASTM D412 |
Lubrizol Estane® L194A Thermoplastic Polyurethane Type: Estane® L194A is a Shore 95A, polyester grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation |
|||
100% Modulus | 0.0137 GPa | 1.99 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR5225 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.0137 GPa | 1.98 ksi | ASTM D-638 |
Axiall 22902 Coax & Telecom Flexible PVC Non-lead stabilized riser jacket recommended over PVC and FRHDPE primaries. Maximum service temperature rating of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |
|||
100% Modulus | 0.0137 GPa | 1.98 ksi | ASTM D-638 |
Axiall 8922 Moldings & Extrusions Flexible PVC A general purpose, matte finish, extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |