Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0131 GPa | 1.90 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.0131 GPa | 1.90 ksi | JIS-A-5756 |
Denka VINYKON W4200 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.0131 GPa | 1.90 ksi | ASTM D-638 |
Axiall 22460 Coax & Telecom Flexible PVC Non-lead stabilized, 75C rated PVC riser jacket over HDPE. Recommended minimum jacket thickness of 22 mils.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0131 GPa | 1.90 ksi | ASTM D-638 |
Axiall 22905 Coax & Telecom Flexible PVC Non-lead tray cable jacket for 75°C maximum service temperature.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0131 GPa | 1.90 ksi | ASTM D-638 |
Axiall 8910 Moldings & Extrusions Flexible PVC Extrusion compound especially formulated for extruded T-moldings, tubings, and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
100% Modulus | 0.0131 GPa | 1.90 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.0131 GPa | 1.90 ksi | ASTM D-638 |
Axiall 54915 Moldings & Extrusions Flexible PVC Medium durometer injection molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |