Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.01079 GPa | 1.565 ksi | -35% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering Perlast® G80S FFKM White Perfluoroelastomer Perlast ® G80S FFKM is a White Perfluoroelastomer 76-85 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and ext.. |
|||
100% Modulus | 0.01079 GPa | 1.565 ksi | ASTM D-638 |
Axiall 14820 Wire & Cable Flexible PVC Non-lead stabilized drop cable jacketing. Also suitable for 80C rated general purpose jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |