Polymer Property : 100% Modulus = 0.009549 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.009549 GPa
1.385 ksi
ASTM D638
Colorite Polymers 7777 Non-Phthalate 77 Series Vinyl Compound
Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio..