Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0093195 GPa | 1.3517 ksi | JIS-A-5756 |
Denka VINYKON M556050 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |