Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00922 GPa | 1.34 ksi | |
C.O.I.M. PLAXTER® P 42 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc. |