Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00904 GPa | 1.31 ksi | |
C.O.I.M. PLAXTER® P 72 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |