Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.008515 GPa | 1.235 ksi | ASTM D412 |
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |