Polymer Property : 100% Modulus = 0.008012 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.008012 GPa
1.162 ksi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ..
100% Modulus 0.008012 GPa
1.162 ksi
ASTM D412
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer
PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra..