Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00765 GPa | 1.11 ksi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-3210 PVC Compound Application: 105°C insulating and jacketing material designed to meet UL 62 for SPT-1 and AWM. UL recognized for QMTT2 TW, THW.Information provided by S&E Specialty Polymers |