Mechanical Properties Metric English Comments
100% Modulus 0.007315 GPa
1.061 ksi
-45% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..