Mechanical Properties Metric English Comments
100% Modulus 0.007067 GPa
1.025 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2121 Fluoroelastomer
3M™ Dyneon™ Flouroelastomer FC 2121 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.007067 GPa
1.025 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2180 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2180 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..