100% Modulus 0.00669 GPa
0.970 ksi
ASTM D638
Colorite Polymers 7884H General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00669 GPa
0.970 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5641Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5641Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..