Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00662 GPa | 0.960 ksi | ASTM D638 |
Colorite Polymers 7000-UV General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00662 GPa | 0.960 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 3075 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00662 GPa | 0.960 ksi | ASTM D638 |
Colorite Polymers 7000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |