Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D638 |
Colorite Polymers 7077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D638 |
Colorite Polymers 7088 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 53080A Moldings & Extrusions Flexible PVC General purpose molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5520 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5520 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00621 GPa | 0.901 ksi | Post Cure 16 Hours @ 232°C |
3M Dyneon™ RA 5300 High Performance Rubber Additive 3M™ Dynamar™ RA 5300 High Performance Rubber Additive is designed for use at low loadings to improve the processing in extrusion and molding operations. It utilizes unique chemistry which makes it.. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 12792 Wire & Cable Flexible PVC General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 14771 Wire & Cable Flexible PVC General purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpor.. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 16782 Wire & Cable Flexible PVC Non-lead stabilized, 90C jacketing compound with excellent low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 873 Wire & Cable Flexible PVC 80°C rated, low migratory, oil resistant coil cord jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 8779 Moldings & Extrusions Flexible PVC Non-lead stabilized, general purpose extrusion compound designed for PVC waterstops per Corps of Engineers Specification CRD-C 572-74.Information provided by Georgia GulfGeorgia Gulf became Axiall C.. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 10750 Wire & Cable Flexible PVC General purpose 75C jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 12780 Coax & Telecom Flexible PVC General purpose coax cable jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 12791 Wire & Cable Flexible PVC General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties and 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall .. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 18750 Wire & Cable Flexible PVC Jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil thickness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in .. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 19750 Wire & Cable Flexible PVC 105°C rated insulation recommended for SPT cord applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D638 |
Colorite Polymers 7002A-02 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 22750 Coax & Telecom Flexible PVC Non-staining extrusion compound recommended for retractile telecommunication cord. Maximum service temperature of 60°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |
|||
100% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D-638 |
Axiall 50898 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |