Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00603 GPa | 0.874 ksi | |
Colorite Polymers Vinylbond 95-950-75 PVC Compound Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri.. |
|||
100% Modulus | 0.00603 GPa | 0.875 ksi | Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2170 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2170 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |