Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00587 GPa | 0.852 ksi | |
Taiwan Sheen Soon Sheenthane® A8550 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00587 GPa | 0.852 ksi | |
Taiwan Sheen Soon Sheenthane® A8700F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00587 GPa | 0.852 ksi | |
Taiwan Sheen Soon Sheenthane® A8870E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00587 GPa | 0.852 ksi | |
Taiwan Sheen Soon Sheenthane® A8871E2 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00587 GPa | 0.852 ksi | |
Taiwan Sheen Soon Sheenthane® A9070A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |