Mechanical Properties Metric English Comments
100% Modulus 0.00565 GPa
0.820 ksi
ASTM D412
Teknor Apex TEKRON® 4300-D90A Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00565 GPa
0.820 ksi
ASTM D412
Teknor Apex UNIPRENE® 7010-87 Thermoplastic Elastomer
Information provided by Teknor Apex Company