Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00564 GPa | 0.818 ksi | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-75A/B Elastomer KEG2000-75 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum.. |