Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00534 GPa
0.775 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00534 GPa
0.775 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00534 GPa
0.775 ksi
ASTM D-638
Axiall 1522 Wire & Cable Flexible PVC
Vinyl elastomer jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00534 GPa
0.775 ksi
ASTM D-638
Axiall 14700 Wire & Cable Flexible PVC
Clear, flexible PVC compound recommended for SPT applications. Maximum service temperature rating of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.