Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00445 GPa | 0.646 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s.. |