Mechanical Properties Metric English Comments
100% Modulus 0.00407 GPa
0.590 ksi
Spartech E65060 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..