Polymer Property : 100% Modulus = 0.00338 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00338 GPa
0.490 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FX 11818 Fluoroelastomer
3M™ Dyneon™ Flouroelastomer FX 11818 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..