100% Modulus 0.00286 GPa
0.415 ksi
Colorite Polymers Vinylbond 95-950-50 PVC Compound
Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri..
100% Modulus 0.00286 GPa
0.415 ksi
ASTM D-638
Axiall 7540 Moldings & Extrusions Flexible PVC
A high quality clear outdoor grade PVC molding and extrusion compound formulated for good UV light resistance and excellent low temperature properties.Information provided by Georgia GulfGeorgia Gul..
100% Modulus 0.00286 GPa
0.415 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 3055 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..