Mechanical Properties Metric English Comments
100% Modulus 0.00269 GPa
0.390 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00269 GPa
0.390 ksi
ASTM D412
Teknor Apex TELCAR® 1050-80 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00269 GPa
0.390 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00269 GPa
0.390 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00269 GPa
0.390 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00269 GPa
0.390 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00269 GPa
0.390 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS